A lining is chosen by what is inside, how hot it runs, how much permeates, and how often you can get back in. Resin choice follows.

Tank lining projects often start with a product name, because someone has used it before or because it is the top of the range. That is the wrong order. The lining has to survive a specific medium at a specific temperature for a specific interval, applied inside a confined space by a crew that may not be able to cure it at the ideal condition. Four questions decide more than any brochure comparison.

The four questions

  • What is inside, at what concentration? Water, brine, acid, alkali, solvent, food product and demineralised water attack coatings in completely different ways. A lining that is excellent in 98% sulphuric acid may be poor in demineralised water, and vice versa.
  • At what temperature, continuous and peak? Chemical resistance tables are quoted at a reference temperature, often 20 or 23 °C. Permeation and reaction rates rise steeply with temperature; a medium that is acceptable at 40 °C can be outside the envelope at 70 °C, and cleaning steam is often the real peak.
  • How much permeates, and is there a vacuum? Solvents and vapours pass through a polymer film and accumulate at the interface. In a tank under negative pressure, that accumulated layer can be pulled off as a blister or a sheet.
  • How is it built and maintained? Carbon steel or concrete, weld quality, ventilation, dew point inside the tank, and how often the tank can be taken out of service. A lining that needs 7 days of cure at 20 °C is a different proposition from one that cures in 24 hours in a cold tank.

What each resin family is good at

Standard epoxy linings are the workhorse: good adhesion, good resistance to water, brine, alkali and many dilute acids, easy to apply at 300–500 µm in two coats. They are not the answer for strong solvents or hot concentrated acids. Novolac epoxy raises temperature and solvent resistance at the cost of a narrower application window. Vinyl ester, often glass-flake filled, handles oxidising acids and hot aggressive media but demands cleaner preparation, tighter mixing control and more careful cure — it punishes shortcuts harder than epoxy does. Polyurethane and flexible linings suit abrasion, low temperature and substrates that move. Where the medium is beyond all of these, the answer is usually brick or tile over a membrane, not a thicker paint.

Thickness is part of the selection, not a detail

A 300 µm lining and a 600 µm lining of the same product are different products in service. Thicker films buy permeation resistance and abrasion resistance; they also buy pinholes, sags on welds, longer cure and higher holiday-test voltages. The thickness must come from the medium and the required life, not from what is convenient to spray in one pass. Two coats are normal for a reason: the second closes the defects of the first.

Where linings fail

Most lining failures are not chemical. They start at a weld spatter that was not ground back, a sharp edge that was not striped, a pinhole that the spark test was set too low to find, or a partially cured film that passed a thumbnail test. The second most common cause is water in the substrate: steel that was blasted the day before, left overnight in humid air, and coated over flash rust. The third is a medium change after commissioning that nobody told the coating supplier about.

Specifying it properly

The specification should carry the medium list with concentrations and temperatures, the required life, the surface preparation grade and profile, the lining thickness per coat, the cure and inspection regime, and the test voltage for holiday detection. Immersion testing of a sample panel in the actual medium is cheap insurance where the chemistry is uncertain. Products such as Interline 850, Tankguard 412 and Chemflake Special sit in different parts of this map — epoxy, solvent-free epoxy and glass-flake vinyl ester respectively — and are not interchangeable even where the datasheet numbers look similar. Whether a given product is suitable for a specific medium at a specific temperature is a question for the manufacturer's chemical resistance guide and the latest TDS; publicly available manufacturer materials are the reference, and a written confirmation for the actual service condition is worth requesting.

The cheapest lining is rarely the one with the lowest price per litre. Compare applied cost per square metre at the specified thickness, add the cost of the inspection and cure time, and then add the cost of being unable to use the tank for an extra week. That comparison usually reorders the shortlist, and it is much easier to do before the purchase order than after the first blister.

Sources

  • ISO 12944-5, public scope (protective paint systems and typical film thicknesses)
  • ISO 12944-9, public scope (offshore and related structures — test methods for protective paint systems)
  • ASTM D471, public scope (rubber property — effect of liquids; widely referenced for immersion testing practice)
  • NACE SP0188 / ISO 29601, public scope (holiday detection and porosity testing)
  • Publicly available manufacturer materials — tank lining and glass-flake vinyl ester ranges and their technical data sheets

Articles are compiled by RichTech from publicly available manufacturer materials and field practice, for selection reference only; the latest official technical data sheets (TDS) prevail.

Not sure which product fits? Tell us the substrate and service conditions

Share your substrate, corrosivity category and target service life — we will come back with a coating system and quantity estimate.

Contact us